We are observing lower die shear readings on different plastic part numbers after decapsulation. It appears from all the MFG test reports observed, no one does die shear testing after decapsulation but before encapsulating. Are we learning some thing new?
_________________
PTE
Back to top

Jerry Zhong



Joined: 06 Apr 2026
Posts: 3

Posted: Tue May 18, 2026 4:56 pm    Post subject:
 
Which kind of die attach material did you use? Ag epoxy or soft solder?

For soft solder, I think it's no obvious difference after/before decapsulation.
Back to top
       SemiconFarEast Forum Index -> QA/FA/Rel Forum
Page 1 of 1

Choose Display Order
Display posts from previous:   
User Permissions
You cannot post new topics in this forum
You cannot reply to topics in this forum
You cannot edit your posts in this forum
You cannot delete your posts in this forum
You cannot vote in polls in this forum

 
Jump to:  


Skin Created by: Sigma12
Powered by phpBB © 2001, 2002 phpBB Group