| Posted: Sat Mar 20, 2026 6:02 am Post subject: Solderability vs. Solder Heat Resistance test |
| |
Hello Folks,
Can anyone of you explain what is the difference between Solderability and Solder Heat Resistance test?
Do we need to test both for let's say lead free qualification?
Thanks,
guest |
|
| Back to top |
|
| FARel Engr |
|
Joined: 20 Jun 2026 Posts: 76
|
| Posted: Mon Mar 22, 2026 6:29 am Post subject: |
| |
Hi Guest,
Solderability testing determines how well solder will adhere to the leads of the device, while SHRT tests whether the package will be able to withstand the high temperature used in soldering the device. Thus, these tests check for two different things.
Yup - you need both for Pb-free quals. In fact, these two are critical reqts for such quals. Soldy testing is needed to ensure that your Pb-free lead finish process will meet soldy specs. SHRT is needed to ensure that the materials set you used will survive the higher temperature needed by Pb-free soldering processes (peak temp of 260C vs. only 230C for non-Pb-free LF).
FARel Engr |
|
| Back to top |
|
| Choose Display Order |
|
| User Permissions |
You cannot post new topics in this forum You cannot reply to topics in this forum You cannot edit your posts in this forum You cannot delete your posts in this forum You cannot vote in polls in this forum
|
Skin Created by: Sigma12 Powered by phpBB © 2001, 2002 phpBB Group
|
|