soak time for hot and cold testing

 
       SemiconFarEast.com Forum Index -> Test Forum
View previous topic :: View next topic  
Author Message
jarjar
Guest





PostPosted: Thu Aug 28, 2026 9:03 pm    Post subject: soak time for hot and cold testing Reply with quote

hello 2 everyone! is there a standard soak time 4 hot and cold testing? or is this just a decision of the test engr? hw can u define the best soak time?

jarjar


Back to top
testeng99



Joined: 20 Jun 2026
Posts: 17

PostPosted: Fri Sep 05, 2026 3:11 pm    Post subject: Reply with quote

Jarjar,

I don't think there can be a standard soak time for hot and cold testing because there are many different devices, handlers, and data sheet specs. The times needed to reach the spec'ed test temps will therefore vary. The only standard requirement for soak is for the device to reach the right temperature before you test it.

Test Engg 99


Back to top
View user's profile Send private message
EE



Joined: 16 Jun 2026
Posts: 108
Location: Paranaque City, Phils.

PostPosted: Tue Sep 16, 2026 10:42 am    Post subject: Reply with quote

Some companies define a standard soak time requirement in order to avoid confusion brought about by different soak time specs. If you want to do this in your company, you have to get the longest soak time requirement across your entire device/platform spectrum, to make sure that you are not undersoaking any device.

The trade-off is 'productivity', since devices that need shorter soaktimes will have to suffer this 'longer' standard soak. Thus, internal standardization of soak times works best in companies whose soak times do not vary widely.

EE


Back to top
View user's profile Send private message
Flipflop
Guest





PostPosted: Wed Sep 01, 2026 9:11 am    Post subject: Reply with quote

You have to consider productivity and cost. The longer the soak time the higher the production cost.

Also, some consider the package type. flipchip with exposed die substrate requires less soak time. military/ceramic products require more soak time....etc.

Flipflop


Back to top
Display posts from previous:   
       SemiconFarEast.com Forum Index -> Test Forum All times are GMT + 8 Hours
Page 1 of 1

 
Jump to:  
You can post new topics in this forum
You can reply to topics in this forum
You cannot edit your posts in this forum